Output of EDGER, American version ================================= entry width [in.]? 5 entry thickness (do not exceed 80% of the width) [in.]? 1 exit width [in.]? 4.5 width reduction is 10.00 % rolling temperature (degrees Fahrenheit, 1560 to 2190)? 1900 actual exit speed [fpm]? 600 roll surface hardness (Shore C, 40 to 100)? 60 for roll material refer to the following table: 0 (Non-graphitic steel); 0.5 (Graphitic steel); 1 (Nodular pearlitic cast iron); 1.5 (Nodular acicular cast iron); 2 (Nodular martensitic cast iron); 2.5 (Chilled cast iron); 3 (IC cast iron); 3.5 (Hi-Chrome cast iron); 4 (Tungsten carbide). roll material? 2 ERT = Equiv. Rect. Thickness Dnom = 13 Dmin = 11.6 Dwor = 12.533 ESA = Exit Section Area rolled stock has C = 1; Mn = 1; Cr = 1 [%] roll pressure = 18899 psi ERT = 1.068 in. roll force = 17 short tons ESA = 4.808 sq.in. roll torque = 4935 ft-lb rotational speed = 183 rpm rolling power = 172 HP forward slip = 0.999 cw = 0.302 m to return to menu, d to exit to DOS